找到了专利摘要(可惜下载不了全文):
PROBLEM TO BE SOLVED: To provide a method of effectively decomposing heavy metals, dioxins, and agricultural chemicals contained in soil, water, seafood, dung of domestic animals, incineration ash, or the like. ; SOLUTION: In this method of decomposing heavy metals, dioxins, and agricultural chemicals, an effective microorganism group containing blended strains comprising 55% aerobic bacteria group and 45% anaerobic bacteria group is mixed with organic waste to carry out a primary fermentation at about 40-200[deg.]C, and, additionally, an effective microorganism group containing blended strains comprising 55% aerobic bacteria group and 45% anaerobic bacteria group is mixed therewith to carry out a secondary fermentation at about 100-200[deg.]C, together with material to be treated, thereby decomposing the heavy metals, dioxins, and agricultural chemicals contained in the material to be treated. ; COPYRIGHT: (C)2003,JPO作者: 倾轻地 时间: 2013-4-20 22:22