小中大【求助】EIS测试的Nyquist数据
EIS测试的Nyquist数据,想用zview拟合,导入数据老是出错,是什么原因呢???
附上数据,求大侠指教啊!!!
1.00E+05 1.61E+00 3.33E-01
7.94E+04 1.59E+00 3.88E-01
6.31E+04 1.55E+00 4.73E-01
5.01E+04 1.57E+00 4.78E-01
3.98E+04 1.60E+00 4.84E-01
3.16E+04 1.63E+00 5.01E-01
2.51E+04 1.65E+00 5.14E-01
2.00E+04 1.67E+00 5.19E-01
1.58E+04 1.70E+00 5.33E-01
1.26E+04 1.73E+00 5.45E-01
1.00E+04 1.76E+00 5.60E-01
7.94E+03 1.80E+00 5.78E-01
6.31E+03 1.83E+00 5.98E-01
5.01E+03 1.87E+00 6.21E-01
3.98E+03 1.92E+00 6.44E-01
3.16E+03 1.96E+00 6.71E-01
2.51E+03 2.01E+00 7.07E-01
2.00E+03 2.05E+00 7.36E-01
1.58E+03 2.11E+00 7.76E-01
1.26E+03 2.17E+00 8.21E-01
1.00E+03 2.23E+00 8.67E-01
7.94E+02 2.30E+00 9.25E-01
6.31E+02 2.38E+00 9.92E-01
5.01E+02 2.46E+00 1.06E+00
3.98E+02 2.56E+00 1.15E+00
3.16E+02 2.67E+00 1.25E+00
2.51E+02 2.78E+00 1.36E+00
2.00E+02 2.92E+00 1.50E+00
1.58E+02 3.10E+00 1.65E+00
1.26E+02 3.28E+00 1.80E+00
1.00E+02 3.53E+00 1.97E+00
7.94E+01 3.80E+00 2.13E+00
6.31E+01 4.10E+00 2.27E+00
5.01E+01 4.46E+00 2.39E+00
3.98E+01 4.86E+00 2.49E+00
3.16E+01 5.25E+00 2.54E+00
2.51E+01 5.64E+00 2.55E+00
2.00E+01 6.07E+00 2.53E+00
1.58E+01 6.49E+00 2.49E+00
1.26E+01 6.79E+00 2.39E+00
1.00E+01 7.12E+00 2.27E+00
7.94E+00 7.42E+00 2.16E+00
6.31E+00 7.69E+00 2.05E+00
5.01E+00 7.94E+00 1.95E+00
3.98E+00 8.17E+00 1.86E+00
3.16E+00 8.38E+00 1.76E+00
2.51E+00 8.58E+00 1.68E+00
2.00E+00 8.77E+00 1.59E+00
1.58E+00 8.94E+00 1.51E+00
1.26E+00 9.12E+00 1.44E+00
1.00E+00 9.27E+00 1.38E+00
7.94E-01 9.42E+00 1.31E+00
6.31E-01 9.56E+00 1.24E+00
5.01E-01 9.69E+00 1.17E+00
3.98E-01 9.80E+00 1.11E+00
3.16E-01 9.92E+00 1.05E+00
2.51E-01 1.00E+01 1.00E+00
2.00E-01 1.01E+01 9.61E-01
1.58E-01 1.02E+01 9.18E-01
1.26E-01 1.03E+01 8.89E-01
1.00E-01 1.04E+01 7.74E-01
7.94E-02 1.05E+01 7.90E-01
6.31E-02 1.06E+01 8.12E-01
5.01E-02 1.08E+01 8.48E-01
3.98E-02 1.09E+01 8.84E-01
3.16E-02 1.10E+01 9.27E-01
2.51E-02 1.12E+01 9.88E-01
2.00E-02 1.14E+01 1.07E+00
1.58E-02 1.16E+01 1.16E+00
1.26E-02 1.19E+01 1.28E+00
1.00E-02 1.22E+01 1.45E+00