Index Frequency (Hz) Z' (Ω) -Z'' (Ω) Z (Ω) -Phase (°) Time (s)
1 99998.5 5.38084 1.00783 5.47441 10.6086 10.6658
2 76093.7 5.29494 0.740788 5.34651 7.96427 12.8727
3 57903.3 5.18229 0.552623 5.21167 6.08684 14.16
4 44061.7 5.15379 0.473123 5.17546 5.2451 15.4269
5 33528.3 5.15947 0.391844 5.17432 4.34309 16.6292
6 25513.6 5.16108 0.332034 5.17175 3.68101 18.8871
7 19414.9 5.18046 0.27823 5.18793 3.07426 20.1947
8 14773.8 5.20594 0.242381 5.21158 2.66569 21.5689
9 11241.9 5.23474 0.214761 5.23914 2.34931 22.8518
10 8554.7 5.26047 0.187117 5.2638 2.03718 25.073
11 6509.66 5.31329 0.179716 5.31633 1.93722 27.3519
12 4953.38 5.34467 0.166495 5.34726 1.78427 28.6487
13 3769.34 5.37754 0.156924 5.37983 1.67149 29.9431
14 2868.24 5.40823 0.153326 5.4104 1.62393 32.0449
15 2182.54 5.43612 0.150246 5.43819 1.58316 33.3183
16 1660.91 5.4584 0.15452 5.46058 1.62153 34.6485
我们测得数据这样,3,4两列你没有啊