小中大PDF#65-5328: QM=Calculated; d=Calculated; I=Calculated
Gallium Manganese Nickel
Ga Mn Ni2
Radiation=CuKa1 Lambda=1.54060 Filter=
Calibration= d-Cutoff= I/Ic(RIR)=11.08
Ref= Calculated from NIST using POWD-12++
Cubic - (Unknown), Fm-3m (225) Z=4 mp=
Cell=5.805 Pearson=cF16 (Bi F3)
Density(c)=8.218 Density(m)=8.20A Mwt=242.06 Vol=195.62 F(19)=999.9(.0002,19)
Ref= Kanomata, T., Shirakawa, K., Kaneko, T.
J. Magn. Magn. Mater., 65 76 (1987)
Strong Line: 2.05/X 1.19/2 1.45/1 0.92/1 1.03/1 0.84/1 3.35/1 1.75/1 2.90/1 1.33/1
NOTE: L 30480 14355 0 TF was not given, B set to 1.000 for calc.
The samples were sealed in evacuated tubes and melted ,then annealed and quenched.The reaction products were pulverized,mixed, heated again in vacuum and then quenched.
EFFECT OF HYDROSTATIC PRESSURE ON THE CURIE TEMPERATURE OF THE HEUSLER ALLOYS Ni2MnZ(Z=Al,Ga,In,Sn AND Sb)
d(A) I(f) I(v) h k l n^2 2-Theta Theta 1/(2d) 2pi/d
3.351 1.3 0.8 1 1 1 3 26.574 13.287 0.1492 1.8747
2.902 0.4 0.3 2 0 0 4 30.780 15.390 0.1723 2.1647
2.052 100.0 100.0 2 2 0 8 44.087 22.044 0.2436 3.0614
1.750 0.6 0.7 3 1 1 11 52.220 26.110 0.2857 3.5898
1.675 0.1 0.1 2 2 2 12 54.730 27.365 0.2984 3.7495
1.451 11.5 16.3 4 0 0 16 64.115 32.057 0.3445 4.3295
1.331 0.2 0.3 3 3 1 19 70.675 35.338 0.3754 4.7180
1.298 0.2 0.3 4 2 0 20 72.800 36.400 0.3852 4.8405
1.184 17.2 29.8 4 2 2 24 81.092 40.546 0.4220 5.3025
1.117 0.1 0.2 5 1 1 27 87.180 43.590 0.4476 5.6242
1.026 4.3 8.6 4 4 0 32 97.288 48.644 0.4872 6.1228
0.981 0.1 0.2 5 3 1 35 103.445 51.722 0.5096 6.4034
0.967 0.1 0.2 6 0 0 36 105.529 52.764 0.5168 6.4942
0.917 5.7 12.7 6 2 0 40 114.116 57.058 0.5448 6.8455
0.885 0.1 0.2 5 3 3 43 120.946 60.473 0.5648 7.0976
0.875 0.1 0.2 6 2 2 44 123.329 61.664 0.5713 7.1797
0.837 1.5 3.7 4 4 4 48 133.654 66.827 0.5967 7.4989
0.812 0.1 0.3 7 1 1 51 142.744 71.372 0.6151 7.7297
0.805 0.1 0.3 6 4 0 52 146.218 73.109 0.6211 7.8051