SGS提供EN 13164挤塑聚苯乙烯泡沫板测试服务 SGS offer EN 13164 Factory made products of extruded polystyrene foam (XPS) Testing Services
Key words: EN 13164, 挤塑XPS, 挤塑苯乙烯, XPS, 绝热材料, 隔热材料, thermal Insulation, thermal conductivity, 导热系数, 热阻, 热阻测试, 隔热, 绝热, 保温, 绝热材料, SGS测试
EN 13164:2012 Thermal insulation products for buildings-Factory made products of extruded polystyrene foam (XPS)- Specification
EN 13164:2012 建筑绝热产品-工厂生产挤塑聚苯乙烯泡沫板-规范
EN 13164标准规范中物理性能测试要求及测试标准如下: For all applications 通用要求
EN 12667(thin) Thermal resistance and thermal conductivity热阻和导热系数
EN 12939(thick)
EN 822 Length and width长度和宽度
EN 823 Thickness厚度
EN 824 Squareness垂直度
EN 825 Flatness 平整度
EN 13501-1 EN 15715 Recation to fire与火反应
For specific applications 特定要求
EN 1604 Dimensional stability尺寸稳定性
EN 1605 Deformation under specific compressive load and temperature conditions特定的温度条件和压缩载荷下的变形
EN 826 Compressive stress or strength压缩应力或压缩强度
EN 1607 Tensile strength perpendicular to faces垂直于表面的拉伸强度
EN 1606 Compressive creep压缩蠕变
EN 12087 Method 2A Long term water absorption长时吸水率
*EN 12088 Long term water absorption by diffusion弥散长时吸水率
EN 12091 Freeze-thaw resistance冻融循环
EN 12086 Water vapour transmission水蒸气传输率
REACH Release of dangerous substances有害物质
EN 13501-1 EN 15715 Recation to fire in standardized assemblies simulating end-use applications 模拟使用环境下的与火反应
*Continuous glowing combustion 持续燃烧
EN 12090 Shear strength剪切强度
Appendix C Ageing procedure for test specimens for the determination of thermal properties老化后热性能
Additional properties 附加性能
EN 12089 Bending strength弯曲强度
EN 13793 Cyclic loading behavior循环载荷测试
EN 826 Compressive modulus of elasticity压缩模量
ISO 4590 Volume percentage of open and closed cells开孔和闭孔体积率